MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik SITREN® AirVoid® 353 Surfactant
Categories: Fluid

Material Notes: Product description: SITREN AirVoid® 353 is a powder antifoam based on organo-modified siloxanes on inorganic carrier.

Applications: SITREN AirVoid® 353 prevents foam formation or destroys foam reliably and may therefore be used in a variety of mortar systems including:

  • Tile adhesives
  • Tile grout mortars
  • Trowelling compounds
  • Repair mortars
  • Renders/stucco
  • Screeds
  • Self-levelling underlayments (SLU)
  • Gypsum-based floor underlayments
Properties/Benefits: As well as excellent foam control properties SITREN AirVoid® 353 provides a variety of additional benefits:
  • Reduction of air in mortars
  • Sustain desired consistency in mortars
  • Excellent long-term stability in dry mortar formulations
  • No negative impact on flow properties
  • No negative impact on set time
  • SITREN AirVoid® 353 can be combined in one formulation at various ratios with SITREN AirVoid® 354 to provide additional benefits as tailor-made air void agents.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.700 - 1.00 g/cc0.0253 - 0.0361 lb/in³
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 4.0 %<= 4.0 %Karl Fischer
 
Descriptive Properties
Appearancegray powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® 383 DS Silica Powder
Evonik SIPERNAT® D 10 Ceramic Powder
Evonik SIPERNAT® 50 Silica Powder
Evonik SIPERNAT® 35 Silica Powder

PEVONIM170 / 197374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.