MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Aero 50/Grade 100 Engine Oil AD
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Aero Engine Oils AD are premium quality ashless dispersant oils for four-stroke aircraft piston engines.

Chevron Aero Engine Oils AD are blended with high quality, high viscosity index base oils, ashless dispersant additives, and antioxidant and antifoam agents.

The ashless dispersant additives retard the formation of sludge and varnish without forming harmful ash deposits in the combustion chamber. The antioxidants resist oxidation, which causes oil thickening and corrosion. The antifoam agent is used to prevent oil foam formation, which can cause unstable oil pressure and loss of oil film strength.

Chevron Aero Engine Oil AD SAE 20W-50 is a multigrade ashless dispersant oil that contains a viscosity modifier that allows for easier startups at low ambient temperatures, while retaining an SAE 50 viscosity at operating temperature.

Applications

Chevron Aero Engine Oils AD are recommended for use in all makes of piston aircraft engines in single and multi-engine light planes and transport-type aircraft.

Chevron Aero Engine Oils AD meet all specification requirements of:

  • Textron Lycoming Specification 301F
  • Teledyne Continental Motors Specification MHS 24
  • Pratt & Whitney Service Bulletin #1183T
Chevron Aero Engine Oils AD meet the requirements of SAE J1899, which has replaced MIL-L-22851D as the standard for ashless dispersant oils.

Key Words: CPS Number: 247507; MSDS Number: 7024
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 29.1 °
Viscosity Measurement 117Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 181 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 18.8 cStASTM D445
Ash 0.00 %Sulfated Ash wt%
 
Thermal PropertiesOriginal ValueComments
Pour Point -27.0 °CASTM D97
Flash Point 248 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Armacell Monarch® F-02001 Neoprene Based Rubber Foam
Low brass, UNS C24000, OSO70 Temper flat products
DuPont Mobility and Materials Neoprene FB Polychloroprene Rubber
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Polychloroprene Rubber (CR)

WCHEV091 / 74706

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.