Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. Bynel® 42E703 is specifically designed for high bonding performance with EVOH in high-speed coextrusion coating or laminating applications. They can also be used in cast film applications. Physical properties of Bynel® Series 4200 resins are typical of low-density polyethylene resins with similar density and melt index values. Information provided by DuPont™ This former DuPont product line is now a Dow product line. |