MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R433H NT0773 PA66-I-GF33
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes: Vydyne R433H NT0773 is general-purpose, heat-stabilized, impact-modified, 33% glass-fiber reinforced PA66 resin. It is specifically designed to maximize toughness, while retaining physical properties. This product is also lubricated for improved flow and offers superior surface appearance.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccDAM; ISO 1183
Water Absorption 1.0 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.3 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 113 MPa50% RH; ISO 527-2
 155 MPaDAM; ISO 527-2
Elongation at Break 4.0 %DAM; ISO 527-2
 6.4 %50% RH; ISO 527-2
Tensile Modulus 6900 MPa50% RH; ISO 527-2
 9400 MPaDAM; ISO 527-2
Flexural Strength 128 MPa50% RH; ISO 178
 220 MPaDAM; ISO 178
Flexural Modulus 5700 MPa50% RH; ISO 178
 8600 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 18.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 19.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 25.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 30.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 99.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 100 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 110 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 110 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 110 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 17.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 18.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 18.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 19.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 25.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 31.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 11.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °CUnannealed; 50% RH; ISO 75-2/B
 259 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 242 °CUnannealed; 50% RH; ISO 75-2/A
 246 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066
 ASTM, D6779
AppearanceNatural Color
FeaturesBalanced Stiffness/Toughness
 Chemical Resistant
 Creep Resistant
 Gasoline Resistant
 Good Dimensional Stability
 Good Heat Resistance
 Good Rigidity
 Good Tensile Strength
 Good Toughness
 Impact Modified
 Lubricated
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9295 / 287645

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.