MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm CyRex® 200-8005 Acrylic-Polycarbonate Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic/Polycarbonate Alloy; Polycarbonate (PC)

Material Notes: CYREX 200-8005 alloy is an opaque, acrylic-polycarbonate alloy with an impact strength that is higher than polycarbonate. Typical properties of CYREX acrylic-polycarbonate alloy are:
  • outstanding impact strength and toughness
  • excellent processing characteristics
  • very good chemical resistance
  • good heat resistance
The special property of CYREX 200-8005 alloy is
  • medium melt flow rate
  • excellent resistance to both alcohol and lipids
  • good resistance to EtO, gamma and E-beam sterilization
Application: Used for injection molding and extrusion of both thin and thick wall applications which require excellent toughness

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Bulk Density 0.650 g/ccASTM D1895
Water Absorption <= 0.26 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cmASTM D951
Melt Flow 3.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 49ASTM D785
Tensile Strength at Break 8000 psiASTM D638
Elongation at Break 57 %ASTM D638
Elongation at Yield 4.3 %ASTM D638
Tensile Modulus 320 ksiASTM D638
Flexural Strength 11300 psiASTM D790
Flexural Modulus 320 ksiASTM D790
Izod Impact, Notched 26.0 ft-lb/in
@Diameter 3.17 mm
bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 52.0 µin/in-°F
@Temperature 0.000 - 100 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 214 °F
@Thickness 6.35 mm
Annealed; ASTM D648
Vicat Softening Point 286 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.0 %Opaque; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 390 - 510 °FCylinder Temp
Melt Temperature 460 - 510 °F
Mold Temperature 150 - 210 °F
Drying Temperature 180 °F
Dry Time 3 - 4 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm CyRex® 200-8000 Acrylic-Polycarbonate Alloy
RTP Company RTP 1800.5A  Polycarbonate/Acrylic Alloy (PC/PMMA) Glass Fiber 5%
Röhm CyRex® 953 Acrylic-Polycarbonate Alloy
304 Stainless Steel
Daicel CEVIAN® CGF20 20% GF PC/Acrylic Alloy

PCYR00043 / 89047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.