MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Zytel® FR70G25V0 NC010 PA66-GF25FR(17)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 25% Glass Reinforced, Flame Retardant, Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³DAM; ISO 1183
Melt Density 1.35 g/cc
@Temperature >=260 °C
0.0488 lb/in³
@Temperature >=500 °F
Water Absorption 3.4 %
@Thickness 2.00 mm
3.4 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 0.900 %
@Thickness 2.00 mm
0.900 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psi50% RH; ISO 527-1/-2
 130 MPa18900 psiDAM; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %DAM; ISO 527-1/-2
 2.6 %2.6 %50% RH; ISO 527-1/-2
Tensile Modulus 7.50 GPa1090 ksi50% RH; ISO 527-1/-2
 9.00 GPa1310 ksiDAM; ISO 527-1/-2
Poissons Ratio 0.340.34DAM; ISO 527-1/-2
 0.340.3450%RH; ISO 527-1/-2
Izod Impact, Unnotched (ISO)  6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 6.50 kJ/m²
@Temperature 23.0 °C
3.09 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched  4.30 J/cm²
@Temperature 23.0 °C
20.5 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+13 ohm1.00e+13 ohm50% RH; IEC 62631-3-2
Dielectric Strength 26.0 kV/mm660 kV/in50% RH; IEC 60243-1
 37.0 kV/mm940 kV/inDAM; IEC 60243-1
Comparative Tracking Index 325 V325 V50% RH; IEC 60112
 350 V350 VDAM; IEC 60112
 250 - 400 V
@Thickness 3.00 mm
250 - 400 V
@Thickness 0.118 in
50% RH; UL 746A
 250 - 400 V
@Thickness 3.00 mm
250 - 400 V
@Thickness 0.118 in
DAM; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 26.0 µm/m-°C14.4 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 83.0 µm/m-°C46.1 µin/in-°FDAM; ISO 11359-1/-2
Specific Heat Capacity 1.91 J/g-°C
@Temperature >=260 °C
0.457 BTU/lb-°F
@Temperature >=500 °F
Melt
Thermal Conductivity 0.220 W/m-K
@Temperature >=260 °C
1.53 BTU-in/hr-ft²-°F
@Temperature >=500 °F
Melt
Melting Point 260 °C500 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 243 °C469 °FDAM; ISO 75-1/-2
Vicat Softening Point 235 °C455 °F50°C/h, 50N; ISO 306
Flammability, UL94  V-0
@Thickness 0.830 mm
V-0
@Thickness 0.0327 in
DAM; IEC 60695-11-10
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
DAM; IEC 60695-11-10
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
DAM; IEC 60695-11-20
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection
 290 °C554 °FInjection Optimum
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FInjection Optimum
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
Emission of organic compounds4.7 µgC/gVDA 277
FMVSS ClassDNIISO 3795 (FMVSS 302)
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Odor4.5VDA 270
Part Marking CodePA66-GF25FR(17)ISO 11469
ProcessingInjection Molding
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPA66-GF25FR(17)ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® FR70G25V0 BK369 PA66-GF25FR(17)
Celanese Zytel® FR70M30V0 NC010 PA66-MD30FR(17)
Celanese Zytel® FR50 NC010 PA66-GF25FR(17)
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Dry)
Celanese Zytel® FR50 BK505 PA66-GF25FR(17)

PDSX5425 / 198065

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.