MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® L 20 HL black 9563 PA12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product Description: Grilamid L 20 HL black 9563 is a, medium viscosity extrusion grade, based on Polyamide 12 (PA12). Grilamid L20 HL black 9563 has been especially developed for external cable sheathing applications, it is UV-stabilized, heat stabilized as it is resistant to termites. The special features of Grilamid L 20 HL black 9563 are:
  • Maximum UV-resistance
  • Heat stability
  • Resistant to termites
  • Good chemical resistance
  • Good resistance to il
  • High surface quality
  • High abrasion resistance
  • Good dimensional stability
  • Easy to process
  • Low density, low weight
Application examples: Grilamid L 20 HL black 9563 is suitable for the outer sheathing layer of telecommunication cables.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³Dry; ISO 1183
Water Absorption 1.5 %1.5 %Sim. to ISO 62
Moisture Absorption 0.700 %0.700 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70
@Time 15.0 sec
70
@Time 0.00417 hour
Conditioned; ISO 868
Tensile Strength at Break 50.0 MPa7250 psiDry; ISO 527-1/-2
 50.0 MPa7250 psiConditioned; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPa5800 psiConditioned; ISO 527-1/-2
 45.0 MPa6530 psiDry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %>= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %Dry; ISO 527-1/-2
 12 %12 %Conditioned; ISO 527-1/-2
Tensile Modulus 1.10 GPa160 ksiConditioned; ISO 527-1/-2
 1.40 GPa203 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mm813 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 550 V550 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C77.8 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C194 - 230 °FLong Term; ISO 2578
 150 °C302 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Fuel systems
 Hydraulic systems
 Powertrain and Chassis
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Tools & Accessories
ProcessingOther Extrusion
Special CharacteristicsImproved heat resistance
 Improved UV resistance (outdoor use)
 Light stabilized or stable to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® L 20 G PA12
Arkema Rilsamid® AESN BLACK P202 T6L PA12-I
EMS-Grivory Grilamid® L 20H FWA black 9225 PA12
EMS-Grivory Grilamid® L 20 GM PA12
EMS-Grivory Grilamid® L 16 W 20 black 9995 PA12

PGRH029 / 156738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.