MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Total PPR 7238 Polypropylene, Random Copolymer - Blow Molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade

Material Notes: Impact Strength. TOTAL Polypropylene 7238 offers excellent impact strength, clarity and gloss.

Lubricated 7238 offers superior core rod release for ease in processing.

High Purity. 7238 features minimum taste, odor, and optimum thermal stability for superior color and processability.

Regulatory. 7238 has passed USP Class VI testing and complies with all applicable FDA and USDA regulations for food contact applications.

Recommended Applications. 7238 is recommended for blow molded containers for food, drug, cosmetic and toiletry applications requiring superior impact strength and clarity.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D1505
Melt Flow 2.0 g/10 minASTM D1238, L
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 23.4 MPaASTM D638
Elongation at Yield 11 %ASTM D638
Tensile Modulus 827 MPaASTM D638
Flexural Modulus 689 MPaASTM D790
Izod Impact, Notched 69.4 J/mASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 143 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
USDA Yes
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion
Dow R132-02A Polypropylene Random Copolymer Resin
Braskem 6D83G Polypropylene Random Copolymer
Total 6232 Polypropylene, Blow Molding Grade
Total PPR 7425 Polypropylene, Injection Molding Grade

PTOTAL839 / 130564

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.