MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance behavior. Carbon additions are optimized in order to provide improved creep resistance properties. Alloy CLI SIRIUS 310 can be easily welded. The alloy is designed for high temperature applications up to 1100°C (2012°F) in oxidizing atmospheres. The alloy can be also used in slightly oxidizing atmospheres,, nitriding, cementing, sulphurising conditions as well as with thermal cyclings, but the maximum temperature of use will be reduced.

Information provided by manufacturer.

Key Words: EN 10095 X8 Cr Ni 25-21 - 1.4845, EN 10028-7 X6 Cr Ni 25-20, AFNOR Z8 CN 25.20, DIN W. Nr 1.4845, ASTM Type 310S
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 550 MPaTypical after Solution Annealing
Tensile Strength, Yield 245 MPa
@Strain 0.2 %
Typical after Solution Annealing
 265 MPa
@Strain 1 %
Typical after Solution Annealing
Elongation at Break 45 %Typical
Creep Strength 120 MPa
@Temperature 600 °C,
Time 3.60e+6 sec
Modulus of Elasticity 200 GPa
Poissons Ratio 0.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000900 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.5 µm/m-°C
@Temperature 20.0 - 100 °C
 16.0 µm/m-°C
@Temperature 20.0 - 200 °C
 17.0 µm/m-°C
@Temperature 20.0 - 400 °C
 18.0 µm/m-°C
@Temperature 20.0 - 600 °C
Specific Heat Capacity 0.480 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Chromium, Cr 25 %
Iron, Fe 54.3 - 54.4 %As remainder
Nickel, Ni 20 %
Silicon, Si 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
310 Stainless Steel, annealed sheet
AISI Type 310S Stainless Steel
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants
Outokumpu 4845 High Temperature Austenitic Stainless Steel
ATI Allegheny Ludlum 310S Austenitic Stainless Steel

NINDUST30 / 17568

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.