MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil CM-P Mobilgrease CM Series
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four products are manufactured with a proprietary high-temperature, lithium complex thickener system. They exhibit excellent resistance to softening under severe working, and provide good adhesion and cohesion. An extreme-pressure additive provides exceptional protection against wear and shock loads, while additional additives enhance resistance to high-temperature oxidation and protection against rust. In addition, Mobilgrease CM-P and Mobilgrease CM-L contain 3% molybdenum sulphide for additional wear protection. Other formulation features provide low-temperature dispensing, very good resistance to water wash, and long service in bearings operating at high temperatures. These heavy-duty, severe-service greases have outstanding structural and chemical stability. Mobilgrease CM Series products will not corrode steel or copper-bearing alloys and are compatible with conventional seal materials. Mobilgrease CM greases are recommended for construction and mining sector applications, as well as heavily loaded industrial bearings. Mobilgrease CM-P is recommended for highly loaded plain and antifriction bearings and other applications where the three percent molybdenum disulphide and high-temperature thickener system will provide good performance. Mobilgrease CM-S is recommended for the lubrication of plain and antifriction bearings in contractor and mining vehicles working under severe operating and weather conditions. The recommended application temperature range for Mobilgrease CM-P and CM-S is -20º C to +175º C Mobilgrease CM-L and CM-W are winter-grade products and are recommended for cold-temperature service. The recommended application temperature range for Mobilgrease CM-L and CM-W is -30º C to +175º C.

The Mobilgrease CM family of products are highly recommended for heavily loaded applications or environments highly contaminated with water, especially in the contractor / mining sector. Specific examples of such applications include: Heavy-duty trucks especially, hinge and bucket pins; Mining and construction equipment; Highly loaded plain and antifriction industrial bearings

Key Words: NLGI Grade 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 320 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.500 mmASTM D2266
Penetration -3.00Penetration Consistency Change, mm/10; ASTM D1831
 280Worked, 25°C, mm/10; ASTM D217
Timken Test >= 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Dropping Point 260 °CASTM D2265
 
Descriptive Properties
Colorgrey
Copper Strip Corrosion, ASTM D40481A
Corrosion Prevention, ASTM D1743pass
Soap/Thickener Typelithium complex
Water Washout, ASTM D1264, wt%6@ 79°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON372 / 75797

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.