MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Anderman Ceramics EC100P Recrystallized Silicon Carbide
Categories: Ceramic; Carbide

Material Notes: EC100P is a porous silicon carbide with excellent thermal shock resistance and high strength and high temperature operating capabilities up to 2910 °F (1600 °C). It is excellent for use in furnaces and molten metal applications due to its non wetting properties. Stock available in tubes, thermocouple sheaths, rods, crucibles and beams.

Key Words: SiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
Open Porosity 15 %
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°C
Maximum Service Temperature, Air 1610 °C
 
Component Elements PropertiesOriginal ValueComments
SiC >= 99.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Silicon Carbide, CVD
Silicon Carbide, sublimed
Morgan Advanced Ceramics CVD Silicon Carbide
CeramTec Rocar® ST Silicon Carbide, SSiC

CANDER13 / 104648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.