MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eagle Brass 102 OF COPPER (Non-Certified), 3/4 Hard
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance and is used for high current applications.

Information provided by Eagle Brass Company

Key Words: UNS C10200, ASTM B152
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³Annealed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 30T 47 - 59Thickness > 0.020 Inch
Tensile Strength, Ultimate 41.0 - 50.0 ksi
Tensile Strength, Yield 39.0 - 48.0 ksi0.2% offset
Elongation at Break 5.0 - 24 %in 2 in.
Tensile Modulus 17000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000176 ohm-cmAnnealed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 2712 BTU-in/hr-ft²-°F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 99.9 %
Oxygen, O <= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oxygen-free high conductivity Copper, Soft, UNS C10200
Eagle Brass 102 OF COPPER (Non-Certified), Annealed
Eagle Brass 101 OFE COPPER (Certified), 1/2 Hard
Eagle Brass 101 OFE COPPER (Certified), Annealed
Eagle Brass 102 OF COPPER (Non-Certified), Hard

NEAGLE012 / 147261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.