MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.

Key Features and Benefits:

  • Self adhesive resin system for sandwich panel applications
  • Flame retardant and self-extinguishing
  • Low tack and long out-times for ease of processing

Applications/Qualifications:

  • Sandwich panels / structures
  • Aircraft Interiors
  • Mass Transit Interiors

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
@Temperature 163 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 70000 psi
@Temperature 23.9 °C
ASTM D638
Tensile Modulus 3800 ksi
@Temperature 23.9 °C
Dry; ASTM D638
Flexural Strength 110 ksi
@Temperature 23.9 °C
Dry; ASTM D790
Flexural Modulus 4300 ksi
@Temperature 23.9 °C
Dry; ASTM D790
Compressive Strength 84.0 ksi
@Temperature 23.9 °C
Dry; ASTM D695
Compressive Modulus 3500 ksi
@Temperature 23.9 °C
Dry; ASTM D695
Shear Strength 8.60 ksi
@Temperature 23.9 °C
Short-Beam, Dry; ASTM D2344
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 93.0 °CDry; DMA
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Climbing Drum Peel (in-lb/3in)45ASTM D1781; Bag Surface
 50ASTM D1781; Mold Surface
Fabric Area Weight (g/m²)300
Prepreg Resin Content (%)37-43
Resin Flow (%)10-25275°F, 15psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARK039 / 89311

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.