MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips EB3300 High Heat Crystal Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Description

Chevron EB3300 is a high molecular weight homopolymer polystyrene that has <200 ppm total residual volatiles content, low gel count and excellent clarity. The high vicat softening point of this resin allows parts produced with this resin to be used at elevated service temperatures. Chevron EB3300 complies with Food Additive Regulation 21CFR177.1640 for polystyrene, which states that such materials may be safely used in contact with foods.

Applications

Typical application for this resin is extruded biaxially-oriented sheet for thermoforming into salad containers, cookie and candy trays, etc.Information provided by Chevron Phillips Chemical Company.

The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Melt Flow 1.7 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8000 psiat 2.0 in/min; ASTM D638
Tensile Strength, Yield 8000 psiat 2.0 in/min; ASTM D638
Elongation at Break 2.5 %ASTM D638
Tensile Modulus 490000 psiASTM D638
Izod Impact, Notched 0.350 ft-lb/in1/4 in.; ASTM D256
 0.400 ft-lb/in1/8 in.; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 197 °FUnannealed specimen; ASTM D648
Vicat Softening Point 227 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene
Ineos Nova 1210 High Heat Crystal Polystyrene
Ineos Nova 1504 High Heat Crystal Polystyrene
Ineos Nova 1510 High Heat Crystal Polystyrene

PPSRA12 / 58242

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.