MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Categories: Polymer; Adhesive

Material Notes:

Features:

  • Alight colored, high strength adhesive with a long tack range
  • Excellent water, oil and grease resistance
  • Bonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 28 - 32 %
Brookfield Viscosity 900 - 1500 cPRVF #2 sp @ 20 rpm @ 80°F
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 68.0 psi
@Temperature 82.0 °C,
Time 1.81e+6 sec
Overlap, 1/8" Birch/Birch
 377 psi
@Temperature 24.0 °C,
Time 1.81e+6 sec
Overlap, 1/8" Birch/Birch
Peel Strength 6.00 pli
@Temperature 24.0 °C,
Time 86400 sec
180°, Canvas/Steel
 10.0 pli
@Temperature 24.0 °C,
Time 259000 sec
180°, Canvas/Steel
 14.0 pli
@Temperature -34.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 22.0 pli
@Temperature 82.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 24.0 pli
@Temperature 66.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 24.0 pli
@Temperature 24.0 °C,
Time 432000 sec
180°, Canvas/Steel
 30.0 pli
@Temperature 24.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 32.0 pli
@Temperature 24.0 °C,
Time 605000 sec
180°, Canvas/Steel
 32.0 pli
@Temperature 24.0 °C,
Time 1.21e+6 sec
180°, Canvas/Steel
 
Thermal PropertiesOriginal ValueComments
Flash Point -26.0 °CTCC
 
Descriptive Properties
AppearanceYellow
BasePolychloroprene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 10 Neoprene Contact Adhesive
COR12V Cork/Neoprene Rubber Sheet
Garlock 3206 Neoprene/Polyester Fabric
Polychloroprene Rubber (CR)
Denka Neoprene 671A Polychloroprene

PMM34116 / 168863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.