MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kazanorgsintez 10803-020 High Pressure Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors.

Application: Intended for production of bags, pipes, fittings, articles designed for food contact, toys, films and film articles, shaped-molded parts, etc.

Information Provided by Kazanorgsintez

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 - 0.920 g/cc
Environmental Stress Crack Resistance >= 2.0 hour
Melt Flow 2.0 g/10 min±10% Superior Quality, ±15% Premium Quality, 2nd Quality
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 9.30 MPa
Elongation at Break >= 550 %
Tear Strength Test >= 12.2MPa
 
Descriptive Properties
Amount of impurities [pcs]152nd Quality
 2Superior Quality
 5Premium Quality
Extractable Substance Weight Content (%)0.9Extra Class
 1.11st and 2nd Class

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kazanorgsintez 11503-070 High Pressure Polyethylene

PKAZAN041 / 127360

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.