MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8254 HS BK-102 PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccdry; ISO 1183
Water Absorption 1.2 %24 hour; ISO Test
 7.1 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.0 %beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.013 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.0 MPa50mm/min; ISO 527
 26.0 MPa2 in/min; ASTM Test
 104 MPa
@Temperature -40.0 °C
ISO Data
 104 MPa
@Temperature -40.0 °C
ASTM Test
Elongation at Break >= 50 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 30 %50mm/min; ISO 527
Tensile Modulus 460 MPa1mm/min; ISO 527
 145 MPa
@Temperature 120 °C
ISO Data
 230 MPa
@Temperature 80.0 °C
ISO Data
 3000 MPa
@Temperature -40.0 °C
ISO Data
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10 K/min
 220 °CASTM Test
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection molding
Mold Temperature 70.0 °CInjection molding
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedYes
Primary Processing TechniqueExtrusion
ProcessingInjection Molding
 Other Extrusion
 Profile Extrusion
Special characteristicHeat stabilized or stable to heat
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
BASF Ultramid® 8253 PA6 (Conditioned)
BASF Ultramid® 8253 HS PA6 (Conditioned)
Envalior Arnitel® EM631-HB TPC-ET
BASF Ultramid® B3K PA6 (Conditioned)

PBASF9176 / 84940

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.