MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 121-67W175 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall or complex profile extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.

Key Features:

  • Recommended for applications requiring excellent flex fatigue resistance.
  • Excellent ozone resistance.
  • Designed for improved UV resistance.
  • Compliant to EU Directive 2003/11/EC regarding marketing and use of certain dangerous substances and preparations, specifically pentabromodiphenyl ether or octabromodiphenyl ether.
  • Designed for extruding thin sections with excellent definition (down to 0.33 mm [0.013"] radius). Long runs with minimal build-up of material on screen packs or narrow die sections.
  • EU and China RoHS compliant
Applications:
  • Automotive- Interior Mat, Seals, Gaskets and Weather Seals
Uses:
  • Automotive Applications
  • Automotive Exterior Trim
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6767.12 in; ASTM D2240
 7171Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 4.279 MPa620.6 psi257°F, 70 hr, in IRM 903 Oil; ASTM D471
 6.64 MPa963 psiAir at 302°F, 168 hr; ASTM D573
 7.38 MPa1070 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 2.96 MPa430 psiAcross Flow; ASTM D412
Elongation at Break 202.5 %202.5 %257°F, 70 hr, in IRM 903 Oil; ASTM D471
 445.5 %445.5 %Air at 302°F, 168 hr; ASTM D573
 450 %450 %Across Flow; ASTM D412
Tear Strength 22.1 kN/m126 pli73°F, Die C; ASTM D624
Compression Set  30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 41 %
@Temperature 125 °C,
Time 252000 sec
41 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.62.6ASTM D150
Dielectric Strength 28.3 kV/mm720 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Die Temperature 204 °C400 °FExtrusion
Melt Temperature 177 - 204 °C350 - 400 °FExtrusion
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Back Pressure 5.00 - 20.0 MPa725 - 2900 psiExtrusion
 
Descriptive Properties
ColorBlack
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-45W255 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer
ExxonMobil Santoprene® 121-40B260 Thermoplastic Vulcanizate Elastomer

PADVA063 / 22753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.