MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lead-Base Babbitt Alloy 13, UNS L53346
Categories: Metal; Nonferrous Metal; Lead Alloy

Material Notes: ASTM B 23 composition specs. Commercially known as mill anchor, chipper babbitt, knife blade.

Key Words: ASTM B 23 (13)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.6 g/ccCalculated
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 19
Tensile Strength, Ultimate 70.0 MPa
Elongation at Break 5.0 %in 50 mm
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb 10 %
Arsenic, As <= 0.25 %
Bismuth, Bi <= 0.010 %
Cadmium, Cd <= 0.050 %
Copper, Cu <= 0.50 %
Lead, Pb 84 %
Tin, Sn 6.0 %
Zinc, Zn <= 0.0050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lead, Pb
Lead-Base Babbitt Alloy 7, UNS L53581 (UNS L53585)
Battery Grid Alloy, Lead-Calcium-Tin (UNS L50740)
Hard Lead (94Pb-6Sb), UNS L53105, Chill Cast
Tin, ASTM B 23 Babbitt Alloy 2 (UNS L13890)

MLB000 / 12206

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.