MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dynasol Calprene® 540 Thermoplastic Rubber SBS Dry
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Calprene 540 is a 60/40 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure. This product is presented in pellet form and has excellent optical properties, due to its clarity. It is stabilized with a non staining antioxidant system FDA approved for use in food contact applications and is essentially gel free with a very clear color. C-540 is used in adhesive formulation, in thermoplastic injected shoe sole formulations, and transparent compounds.

Applications:

  • Footwear
  • Adhesives
  • Plastic modification

Information provided by Dynasol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.40 %ASTM D-5668
Viscosity 600 cP25% toluene solution; MA 04-3-064
Brookfield Viscosity 1100 cP25% toluene solution; MA 04-3-064
Melt Index of Compound 5.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D-1238
Ash <= 0.35 %ASTM D-5667
 
Chemical PropertiesOriginal ValueComments
Styrene Content 40 %on polymer; ASTM D-5775
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D-2240
Abrasion 100mm³; DIN 53516
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Hunterlab color, max3
Insolubles in toluene, 325 mesh, % max0.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dynasol Calprene® H6120 Hydrogenated Rubber SEBS
Dynasol Calprene® 501 Thermoplastic Rubber SBS Dry
Dynasol Calprene® H6215 Hydrogenated Rubber SEBS
Dynasol Solprene® 411 Thermoplastic Rubber SBS Dry
Dynasol Calprene® H6170 Hydrogenated Rubber SEBS

PDYNA52 / 34798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.