MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
E-Polymers TEKALOY® F50G50 50% Glass Fiber Reinforced PBT/PET Alloy
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polyethylene Terephthalate (PET)

Material Notes: PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability. PC/PBT is usually used for automotive applications with good resistance against oils and solvents as well as high impact. PC/PET has an excellent surface and its high heat resistance allows it to be employed in housing for electrical appliances.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.73 g/ccASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 156.96 MPaASTM D638
Elongation at Break 1.5 %ASTM D638
Flexural Strength 245.25 MPaASTM D790
Flexural Modulus 16190 MPaASTM D790
Izod Impact, Notched 10.0 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 225 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 300 °C
Mold Temperature 80.0 - 100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Optical Grade
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET
Overview of materials for Nylon 6, Extruded
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural
Lotte Advanced Materials Infino® EN-1052 PC, FR

PEPOLZ041 / 103538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.