MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EDRO #8 Premium 420 Stainless Mold Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in hardening.
EDRO #8™ is recommended for all types of molding tools, its special properties make it particularly suitable for molds with the following demands: corrosion/staining resistance, i.e., for molding of corrosive materials, e.g. PVC, acetates, and for molds subjected to humid working/storage conditions; Wear resistance, i.e., for molding abrasive/filled materials, including injection-molded thermosetting grades - also for molds with exceptionally long production runs, e.g. electrical/electronic parts; disposable cutlery and containers; High surface finish, i.e., for production of optical parts, such as camera and sunglass lenses, and for medical containers, e.g. syringes, analysis phials.
EDRO #8™ is resistant to corrosive attack by water, water vapor, weak organic acids, dilute solutions of nitrates, carbonates and other salts.

Information provided by EDRO

Key Words: AISI 420 improved, W.-Nr 1.2083
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.277 lb/in³
@Temperature 399 °C
Hardened and tempered to 50 HRC
 0.280 lb/in³
@Temperature 199 °C
Hardened and tempered to 50 HRC
 0.282 lb/in³
@Temperature 20.0 °C
Hardened and tempered to 50 HRC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 215Delivery condition (soft annealed)
Hardness, Rockwell C 38
@Treatment Temp. 566 °C
Tempered twice for 2 hr at temperature
 50
@Treatment Temp. 482 °C
Tempered twice for 2 hr at temperature
 52
@Treatment Temp. 177 °C
Tempered twice for 2 hr at temperature
 53
@Treatment Temp. 260 °C
Tempered twice for 2 hr at temperature
 55
@Treatment Temp. 399 °C
Tempered twice for 2 hr at temperature
 55
@Treatment Temp. 93.3 °C
Tempered twice for 2 hr at temperature
Tensile Strength, Ultimate 206000 psi45 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
 256000 psi50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
 300000 psi55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
Tensile Strength, Yield 185000 psi45 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
 213000 psi50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
 234000 psi55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
Elongation at Yield 8.0 %in 2", 55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
 10 %in 2", 50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
 12 %in 2", 45 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
Reduction of Area 27 %55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
 30 %50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
 40 %45 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
Modulus of Elasticity 27500 ksi
@Temperature 399 °C
 30400 ksi
@Temperature 199 °C
 31100 ksi
@Temperature 20.0 °C
Izod Impact 12.0 ft-lb
@Treatment Temp. 510 °C
Tempered for 2 hr
 15.0 ft-lb
@Treatment Temp. 371 °C
Tempered for 2 hr
 15.0 ft-lb
@Treatment Temp. 149 °C
Tempered for 2 hr
 20.0 ft-lb
@Treatment Temp. 260 °C
Tempered for 2 hr
 24.0 ft-lb
@Treatment Temp. 649 °C
Tempered for 2 hr
 55.0 ft-lb
@Treatment Temp. 760 °C
Tempered for 2 hr
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.10 µin/in-°F
@Temperature 20.0 - 199 °C
 6.40 µin/in-°F
@Temperature 20.0 - 399 °C
Specific Heat Capacity 0.110 BTU/lb-°F
@Temperature 20.0 °C
Thermal Conductivity 159 BTU-in/hr-ft²-°F
@Temperature 20.0 °C
 166 BTU-in/hr-ft²-°F
@Temperature 199 °C
 173 BTU-in/hr-ft²-°F
@Temperature 399 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.38 %
Chromium, Cr 13.6 %
Iron, Fe 84.42 %As Balance
Manganese, Mn 0.50 %
Silicon, Si 0.80 %
Vanadium, V 0.30 %
 
Descriptive Properties
Color CodeBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
420 Stainless Steel
304 Stainless Steel
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel
316 Stainless Steel, annealed strip
Kinetics MIM 420 Stainless Steel (Oil Quench Heat Treat)

NSEDRO008 / 142945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.