MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dental Amalgam
Categories: Metal; Nonferrous Metal; Precious Metal

Material Notes: This silvery-white alloy is used frequently as dental fillings. It is composed mainly of intermetallics Ag3Sn and Ag2Hg3 with Sn7Hg or Cu6Sn5 (depending on Cu content).

Key Words: Fillings; Mercury Alloys
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.0 g/cc0.397 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 9090
Tensile Strength, Ultimate 30.0 - 60.0 MPa4350 - 8700 psiWide range is possible
Tensile Modulus 60.0 GPa8700 ksi
Compressive Yield Strength 275 - 345 MPa39900 - 50000 psiafter five days
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.0 - 28.0 µm/m-°C
@Temperature 37.0 °C
12.2 - 15.6 µin/in-°F
@Temperature 98.6 °F
near body temperature.
Shrinkage -0.200 - 0.20 %
@Temperature 23.0 °C
-0.200 - 0.20 %
@Temperature 73.4 °F
During Hardening
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 2.0 - 15 %2.0 - 15 %
Mercury, Hg 40 - 50 %40 - 50 %
Silver, Ag 20 - 35 %20 - 35 %
Tin, Sn 12 - 15 %12 - 15 %
Zinc, Zn <= 1.0 %<= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade
Kennametal Stellite Denertia™ N8 Nickel Dental Alloy
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2

MPHg00 / 12547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.