MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion Alloy 10X CuCoBeZr Alloy, TH04 Temper
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Alloy 10X is a copper-cobalt-beryllium-zirconium alloy developed for improved high temperature strength and ductility compared to most copper alloys. Alloy 10X retains good strength and ductility at temperatures up to 800°F/430°C. With its combination of good elevated temperature strength and conductivity, it has superior resistance to thermal cracking. It is the copper alloy of choice for operation above 575°F/300 °C where high strength is required.

Information supplied by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.83 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B >= 92
Tensile Strength, Ultimate 515 MPa
@Temperature 427 °C
 >= 690 MPa
@Temperature 20.0 °C
Tensile Strength, Yield 450 MPa
@Strain 0.2 %,
Temperature 427 °C
 >= 585 MPa
@Strain 0.2 %,
Temperature 20.0 °C
Elongation at Break 5.0 %
@Temperature 427 °C
 >= 15 %
@Temperature 20.0 °C
Modulus of Elasticity 138 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000310 - 0.00000380 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.6 µm/m-°C
Specific Heat Capacity 0.414 J/g-°C
Thermal Conductivity 225 W/m-K
Melting Point >= 1010 °C
Solidus 1010 °C
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.40 - 0.70 %
Chromium, Cr <= 96.2 %
Cobalt, Co 2.0 - 2.7 %
Copper, Cu >= 97.5 %As Balance
Zirconium, Zr 0.12 - 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410)
Beryllium Copper Alloy 10C, UNS C82000 As-cast
Brush Wellman Beryllium Copper Alloy 165 Strip; 1/2H (TD02) Temper (UNS C17000)
Brush Wellman Beryllium-Copper Alloy 171 1/2 HT (TH02) Temper
Brush Wellman Beryllium-Copper Alloy 171 1/4 HT (TH01) Temper

NBB401 / 192241

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.