MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ALM HT-23 PEKK, 23% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; PEKK, Reinforced

Material Notes: The HT-23 is based on a PEKK resin with 23% Carbon Fiber compounded in and ground to a fine powder.

Highlights:

  • Isotropic properties
  • Melt compounded Carbon Fiber filled PEKK
  • High melt point
  • Chemical resistant
  • Inherently flame retardant
Applications:
  • Aerospace
  • Mobility industry
  • Complex geometries requiring accuracy and feature resolution
  • Well suited to applications which require superior thermal properties, with maximum performance and consistent properties in XY&Z dimensions

Information provided by Advanced Laser Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 g/cc0.0181 lb/in³ASTM D1895
Density 1.39 g/cc0.0502 lb/in³Sintered; ASTM D792
Particle Size 80 µm80 µmD50
 45 - 115 µm45 - 115 µmD10-D90
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 350 °C
20 g/10 min
@Load 4.76 lb,
Temperature 662 °F
5 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 61.0 MPa8850 psiZ; ASTM D638
 77.0 MPa11200 psiY; ASTM D638
 80.0 MPa11600 psiX; ASTM D638
Tensile Strength, Ultimate 59.0 MPa8560 psiZ; ASTM D638
 71.0 MPa10300 psiXY; ASTM D638
Elongation at Break 1.06 %1.06 %Z; ASTM D638
 1.1 %1.1 %Z; ASTM D638
 1.16 %1.16 %XY; ASTM D638
 1.3 %1.3 %X; ASTM D638
 1.3 %1.3 %Y; ASTM D638
Tensile Modulus 5.80 GPa841 ksiZ; ASTM D638
 6.40 GPa928 ksiY; ASTM D638
 6.50 GPa943 ksiX; ASTM D638
Flexural Strength 81.0 MPa11700 psiZ; ASTM D790
 101 MPa14600 psiXY; ASTM D790
Flexural Modulus 5.13 GPa744 ksiZ; ASTM D790
 5.97 GPa866 ksiXY; ASTM D790
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inXY; ASTM D256
 1.01 J/cm1.89 ft-lb/inZ; ASTM D256
Izod Impact, Unnotched 0.180 J/cm0.337 ft-lb/inZ; ASTM D256
 0.200 J/cm0.375 ft-lb/inXY; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.28e+14 ohm-cm1.28e+14 ohm-cmX, 50%RH, 500V; ASTM D257
 2.08e+14 ohm-cm2.08e+14 ohm-cmZ, 50%RH, 500V; ASTM D257
 3.83e+14 ohm-cm3.83e+14 ohm-cmY, 50%RH, 500V; ASTM D257
Surface Resistivity per Square 5.38e+11 ohm5.38e+11 ohmY, 50%RH, 500V; ASTM D257
 1.46e+14 ohm1.46e+14 ohmX, 50%RH, 500V; ASTM D257
 1.68e+15 ohm1.68e+15 ohmZ, 50%RH, 500V; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 302 °C576 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 274 °C525 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 202 °C396 °FASTM D648
 
Descriptive Properties
ColorDark Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALP9010 / 312345

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.