MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Bormed HF855MO is a high modulus polypropylene homopolymer and is especially developed within the proprietary Borstar technology. Bormed HF855MO combines an unique balance of properties for high speed injection molding allowing fast cycle time due to high de-molding temperature as well as reduced cooling time.

Bormed HF855MO is designed for containers and products with medium to long flow lengths, rectangular and flat products, pharmaceutical and diagnostic packaging, and syringe plungers.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ISO 2039-2
Tensile Strength, Yield 40.0 MPaAt 50 mm/min; ISO 527-2
Elongation at Yield 6.0 %At 50 mm/min; ISO 527-2
Tensile Modulus 2.20 GPaAt 1 mm/min; ISO 527-2
Charpy Impact, Notched 0.250 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 122 °CISO 75-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °C
Mold Temperature 30.0 - 60.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications
Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications
Borealis Bormed™ RG835MO Polypropylene Copolymer for Healthcare Applications
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications
Total PPH 3620WZ Polypropylene, Injection Molding Grade

PBOREA075 / 27382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.