MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
40Pt-60Pd Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy

Key Words: Platinum Palladium Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 15.8 g/ccCalculated from pure elements
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 101Estimated from Vickers
Hardness, Knoop 114Estimated from Vickers
Hardness, Rockwell B 54Estimated from Vickers
Hardness, Vickers 100
 175Hard heat treatment
Tensile Strength, Ultimate 350 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000270 ohm-cmTemperature Coefficient = 0.001/K
 
Component Elements PropertiesOriginal ValueComments
Palladium, Pd 60 %
Platinum, Pt 40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
80Pd-20Ag Alloy, Annealed
77Pd-23Ag Palladium Silver Alloy
75Pd-25Ag Palladium Silver Alloy
70Pd-30Ag Palladium Silver Alloy
60Pd-40Cu Alloy, Hard Drawn

MPPtP2 / 12589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.