MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton 662 FG Barrier Fluid 22
Categories: Fluid; Lubricant; White Mineral Oil (WMO)

Material Notes: Chesterton® 662 FG is an ISO grade 22, high-performance lubricant designed specifically for mechanical seal applications. Dual mechanical seals rely on a premium grade lubricant to ensure greatest mean-time-between-failure, safe operation and to avoid product contamination. The 662 FG is a non-toxic lubricant that delivers superior heat transfer properties optimizing the seal environment. 662 FG does not contain dyes, additives, or heavy metals that could contaminate process streams or poison catalytic systems. The ultra clean 662 FG is designed to deliver premium thermal stability while minimizing abrasive particle wear of the seal faces and provide long life.

Features:

  • Clear, colorless, odorless
  • Convenient to use
  • High performance value
  • Cost effective
  • Saves time and labor
  • Superior heat transfer capabilities
  • High purity
  • Wide temperature range
  • Compatible with most fluids(mineral oil, PAO and Diester) (not miscible with glycols or silicones)
  • NSF H1 Registration number 143837

Applications: Bearings and mechanical seals have the tightest tolerances within a typical pump. The mechanical seal utilizes ultra flat sliding seal faces to make a reliable seal. As with bearings, mechanical seals require a clean stable lubricant to maximize performance. The 662 FG high performance formulations in combination with Chesterton’s high performance mechanical seals offer the most reliable dual seal package on the market today. Chesterton 662 FG has been extensively tested and designed to be compatible with common seal material use in industry. Designed for optimized performance in mechanical seals, this lubricant improves seal performance with or without pumping rings.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 g/cc
Kinematic Viscosity at 40°C (104°F) 22 cSt
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
Vapor Pressure <= 36.8 torr
@Temperature 500 °C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.96 J/g-°C
@Temperature 50.0 °C
 2.38 J/g-°C
@Temperature 500 °C
Thermal Conductivity 0.115 W/m-K
@Temperature 500 °C
 0.133 W/m-K
@Temperature 50.0 °C
Boiling Point 358 °C
Pour Point -40.0 °CASTM D97
Flash Point 171 °CASTM D92
Ignition Temperature 346 °CAutoignition
 
Descriptive Properties
AppearanceClear, Liquid
BaseHydrotreated White Mineral Oil
Fire Point232°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Packers Oil
ChevronTexaco Superla® 50 White Oil
ChevronTexaco TEGRA® ISO 32 Synthetic Compressor Oil
ChevronTexaco Snow White Petrolatum
ChevronTexaco Regal® 32 R&O

PPTCHS066 / 138178

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.