MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow FUSABOND™ N525 Anhydride-Modified Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene

Material Notes: Product Description: FUSABOND™ N525 is an anhydride modified ethylene elastomer.
Uses: Polymer Modifier
Composition:
  • High% by weight maleic anhydride
  • Graft levels are defined as:
  • Low <0.2%; Medium 0.2-0.5%; High 0.5-1.0%; Ultra high >1.0%
Applications:
  • Impact modifier for polyamide blends with high MAH grafting level
  • Efficient modifier for polyolefin based wire and cable compounds
  • Blends for golf balls covers
  • Compatibilizer or adhesion promoter between polyolefins and metals, polyamide, cellulose, and glass fibers.
Availability: Africa & Middle East; Asia Pacific; Europe: Latin America; North America

Additive: Impact Modifier

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccISO 1183
 0.882 g/ccASTM D792
Melt Flow 3.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 3.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30ASTM D2240
Tensile Strength at Break 870 psi
@Temperature 22.8 °C
Type IV, 20 in/min; ASTM D638
 2030 psi
@Temperature 20.0 °C
Type IV, 2.0 in/min; ASTM D638
Tensile Stress 870 psi
@Temperature 22.8 °C
Type IV, 20 in/min; ISO 527-2/500
 2030 psi
@Temperature 20.0 °C
Type IV, 2.0 in/min; ISO 527-2/50
Elongation at Break 550 %
@Temperature 22.8 °C
Type IV, 20 in/min; ASTM D638
 590 %
@Temperature 22.8 °C
Type IV, 2.0 in/min; ASTM D638
Flexural Modulus 3190 psi0.05 in/min; ASTM D790
 3190 psi0.05 in/min; ISO 527-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 108 °FFreezing point
 136 °F
Vicat Softening Point 108 °FASTM D1525
 108 °FISO 306
Glass Transition Temp, Tg -56.2 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF540 / 311233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.