MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive
Categories: Polymer; Adhesive

Material Notes: Self-extinguishing version of 3748. Meets UL 1410 requirements

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/cc
Viscosity 3300 cP
@Temperature 220 °C
 5000 cP
@Temperature 200 °C
 8500 cP
@Temperature 180 °C
Brookfield Viscosity 5500 cP
@Temperature 191 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 26ASTM D2240
Shear Strength 215 psiFR-24 to FR-4
 220 psiPE to PE
 250 psiPP to PP
 275 psiOn Douglas Fir
 275 psiFirt to Fir
Peel Strength 15.0 plion canvas
 26.0 pliFir, 180°
 27.0 pliPE, 180°
 35.0 pliPP, 180°
 38.0 pliWire Mesh to FR-4, 180°
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+17 ohm-cmASTM D257
Surface Resistance 4.50e+17 ohm
Dielectric Constant 2.3
@Frequency 100 - 1.00e+8 Hz
ASTM D149
Dielectric Strength 1400 kV/in
@Thickness 0.279 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 1000 - 1.00e+8 Hz
ASTM D149
 0.0020
@Frequency 100 Hz
ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear -3.40 µm/m-°C
@Temperature -40.0 °C
 15.4 µm/m-°C
@Temperature 25.0 °C
Thermal Conductivity 1.92 W/m-K
Flammability, UL94 V-0
Ring & Ball Softening Point 152 °CASTM E28-99

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 3750 Tan Hot Melt Adhesive
3M Scotch-Weld™ 3764 Hot Melt Adhesive
3M Scotch-Weld™ 3731 Hot Melt Adhesive
3M Scotch-Weld™ 3748 Hot Melt Adhesive
3M Scotch-Weld™ 3747 Hot Melt Adhesive

PMM34090 / 168837

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.