MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOMER® DA 850 Polymeric copolymer
Categories: Other Engineering Material

Material Notes: Product description: TEGOMER® DA 850 is a polymeric copolymer with pigment affinic groups to be used as a dispersant in water based-surroundings.

Application: TEGOMER® DA 850 is a liquid dispersing additive used in the manufacturing of water-based pastes of:

  • inorganic fillers e.g. talc or barium sulfate, chalk
  • inorganic pigments e.g. titanium dioxide, ultramarine blue, iron oxides
  • organic pigments and carbon blacks
Benefits: The use of TEGOMER® DA 850 offers several advantages:
  • higher filling of pastes
    • excellent rheological properties even during long-term storage of pastes
    • prevention of hard settlement of fillers and pigments with high density, e.g. titanium dioxide or barium sulfate
    • improved color strength and covering power
    • less speck formation or agglomerates
    • reduced abrasion properties on the doctor blade used for the application of finishes
    • improved mechanical properties
    • improved durability
    • solvent and nonylphenol ethoxylate-free

    Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 6.0 - 7.5
Viscosity 100 - 500 cP
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.39 - 1.405
Gardner Color Number 5.0
 
Descriptive Properties
Appearanceliquid, clear, slightly yellowish colored
Content38-42%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Latex XZ 92229.03 Experimental Latex
Solvay RHODASURF® LA-985 Surfactant
Solvay RHODASURF® LA-23/6.5 Surfactant
Solvay RHODAFAC® RS-710 Surfactant
Solvay RHODAFAC® ASI 80 BC Surfactant

PEVONIL582 / 196786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.