MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Delrin® 500PE BK602 POM  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Medium Viscosity Acetal Homopolymer with Very Low Emissions

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccISO 1183
Melt Density 1.20 g/cc
@Temperature >=178 °C
Water Absorption 0.90 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cmISO 294-4, 2577
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
from MVR and melt density; ISO 1133
 14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 93ISO 2039-2
Hardness, Rockwell R 121ISO 2039-2
Tensile Strength, Yield 73.5 MPaISO 527-1/-2
Elongation at Break 27 %ISO 527-1/-2
Elongation at Yield 13 %ISO 527-1/-2
Tensile Modulus 3350 MPaISO 527-1/-2
Flexural Yield Strength 85.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 3150 MPaISO 178
Poissons Ratio 0.37ISO 527-1/-2
Charpy Impact Unnotched 225 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 250 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohmIEC 62631-3-2
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.9
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 43.0 kV/mmIEC 60243-1
Dissipation Factor 0.00050
@Frequency 100 Hz
IEC 62631-2-1
 0.0055
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CISO 11359-1/-2
 90.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-1/-2
 90.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 159 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 103 °CISO 75-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 210 °CInjection
 205 °CInjection Optimum
Mold Temperature 80.0 - 100 °CInjection
 90.0 °CInjection Optimum
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %Injection
Hold Pressure 80.0 - 100 MPaInjection
Annealing Temperature 160 °CInjection
 
Descriptive Properties
Annealing time30 min/mmInjection - Optional
Delivery formPellets
Drying RecommendedyesInjection
Emissions<2 mg/kgVDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging G-value (condensate) (mg)0.35ISO 6452
Hold pressure time (s/mm)8Injection
Part Marking CodePOMISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPOMISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 100STE NC010 POM-HI
Delrin Delrin® 500TL NC010 POM-SD
DuPont Mobility and Materials Delrin® 100PE NC010 POM
Delrin Delrin® 500T BK602 POM-I
Delrin Delrin® 500P BK602 POM

PDSX5120 / 197760

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.