MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Texclad® 2
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Texaco Texclad 2 delivers value through:
  • Water tolerance — Resists washout, even when subject to gross water contamination.
  • Excellent adhesiveness — Assures good film strength even in a wet environment.

Texaco Texclad 2 is calcium-based grease, which contains special functional fillers such as molybdenum disulfide and graphite, which impart a long-lasting film on working surfaces. Texclad has good load carrying capability and is very resistant to water washout.

Texaco Texclad 2 additive system includes friction modifiers such as molybdenum disulfide and graphite, which apply a long lasting antiwear film on lubricated surfaces.

Texaco Texclad 2 is recommended:

  • For ball mill gears, traveling water screens, and fork lifts.
  • For chain and sprocket lubrication and as a tenacious fifth wheel lubricant.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 221956; MSDS Number: 9008

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 875 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 36.5 cStSee Note 3.
 
Mechanical PropertiesOriginal ValueComments
Penetration P(60), 1/10 mm 280Unknown Amount of Work, 25°C (77°F)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 79.0 °CSee Note 2.
Minimum Service Temperature, Air -18.0 °CSee Note 1.
Dropping Point 232 °C
 
Descriptive Properties
ColorBlack
TextureTacky
Thickener, %9Calcium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA275 / 77154

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.