System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Buckeye Polymers BP RPP 2009 GK BLK Polypropylene, 20% Glass Filled
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 20% Glass Fiber Filler
Material Notes:
Product Information:
Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced engineering thermoplastics in numerous applications.
Product Features:
Good flexural strength
Appearance:
Black
Forms:
Pellets
Processing Method:
Injection Moulding
Information Provided by Buckeye Polymers, Inc.
Key Words:
glass content 16-22%
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Carbon Black Loading
1.0 %
Melt Flow
2.0
-
12
g/10 min
ASTM D1238
Ash
16 - 22 %
ASTM D5630
Mechanical Properties
Original Value
Comments
Flexural Modulus
>=
216775
psi
ASTM D790
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
LG Chemical LUPOL GP-2201F General Purpose Polypropylene, 20% Glass Fiber Reinforced, Flame Retardant
LG Chemical LUPOL GP2150 PP+GF15%
E-Polymers TEKAFINĀ® PH50G2 20% Glass Fiber Reinforced High Strength Compounded-PP
Cossa Polimeri ESTAPROP H 0540 GFC Polypropylene, 20% Glass Filled
Cheng Yu Plastic PP237G2 Polypropylene, 20% Glass Fiber
PBUCK011 / 104479
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.