MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond FLM36-LO Film Adhesive
Categories: Polymer; Adhesive; Film

Material Notes: Key Features:
  • High temperature resistant
  • Thermally conductive
  • Tough and flexible
  • Easy to apply and doesn’t require freezing
  • Excellent electrical insulation properties
  • Uniform bond line thickness
Product Description: Master Bond FLM36-LO is a very special film adhesive featuring incomparable strength properties, high temperature resistance and first class thermal conductivity and electrical insulation properties. Functionally, it is similar to EP36AO and both that product and this film differ from other heat resistant epoxies as they possess far more toughness and flexibility than conventional high temperature epoxies. This highly unusual system has a relatively low glass transition temperature, and although softer above it, FLM36-LO retains its very high physical strength properties profile up to 500°F. Ultimately, FLM36- LO combines markedly enhanced thermal and mechanical shock resistance and thermal cycling capabilities. FLM36- LO bonds well to a variety of substrates including metals, composites, glass and many plastics. It has good chemical resistance to water, acids, bases, fuels and oils. The service temperature range is -100°F to +500°F. Being a film, it, of course, doesn’t require any mixing. The processing is very straightforward, that is heat curing at 350°F for 1-2 hours in order to obtain optimal properties. Two outstanding and highly desireable features of FLM36-LO include its uniformity of bond line thicknesses and limited squeeze out during the bonding process. An additional noteworthy characteristic is its low outgassing conformity to the NASA ASTM E595 specification. This product is offered in three standard sizes: FLM36- LO-4A is 4 x 4 x 0.008 inches, FLM36-LO-8B is 8 x 8 x 0.008 inches and FLM36-LO-12C is 12 x 12 x 0.006 inches. The film can be cut with a pair of scissors into various shapes and sizes. With intricate shapes, preforms can be provided; although, a technical drawing with tolerances would be required. The films are rugged, durable and not prone to cracking. Using the film is simple. The films have release paper on each side. After the substrates are surface prepared, the release paper is removed on one side to expose the adhesive. It’s carefully placed onto the part and pressure is applied. The film is adhering to the surface as it possesses a “tackiness” to it. The second release lining is removed and the other substrate is affixed accordingly. The assembly is lightly fixtured and cured for 1-2 hours at 350°F. The bonded parts should be returned to 75°F before removing the fixtures. The film is black in color to provide a vivid contrast from the release papers. Unlike nearly all the thermoset films of this type, FLM36-LO does not require freezing, although refrigeration is recommended. The plethora of advantages in using this film with its unique flexibilized epoxy chemistry is that it offers high temperature resistance, extraordinary toughness and flexibility, the ability to withstand rigorous thermal cycling and the distinction of complying with NASA low outgassing criteria. These properties enable it to be an excellent candidate for aerospace, electronic, opto-electronic, specialty OEM and applications requiring vacuum compatibility. Also, its thermal conductivity and electrical insulation properties are integral constituents of the product property profile of FLM36-LO.

Product Advantages:

  • Provides uniform bond line thicknesses, virtually no squeeze out when curing
  • Exceptionally rugged; easily cut into shapes
  • Black color facilitates application; cures readily at 350°F for 1-2 hours
  • After polymerization it combines high temperature resistance with flexibility and toughness
  • Withstands aggressive thermal cycling
  • Meets low outgassing specification

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 22
@Temperature 177 °C
 27
@Temperature 100 °C
 80
@Temperature 23.9 °C
Tensile Strength >= 2000 psi
Elongation at Break >= 50 %
Adhesive Bond Strength >= 4000 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 75.0 - 85.0 µm/m-°C
Thermal Conductivity 9.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -100 °F
Glass Transition Temp, Tg 30.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 177 °C
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
in original, unopened containers
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond FLM36 B-staged film for high performance bonding and sealing
Carlson 90 10 Cu Ni Copper-Nickel Alloy
Carlson 70 30 Cu Ni Copper-Nickel Alloy
304 Stainless Steel
302 Stainless Steel, annealed strip

PMASTM918 / 185511

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.