MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay P720X PET-Based Release Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Description: Release film. Ideally suited to quasi-istropic applications.

Features & Benefits:

  • Matte finish film with high modulus and low elongation providing a flat contact surface that is compatible with most commonly used resin systems and adhesives
  • Excellent for use as a backing film for automated or manual tape laying of quasi-istropic lay-ups that will subsequently be transferred to an automated cutting table for final dimension cutting
  • Although capable of high temperature, P720X is not intended for use as a release film above 93°C (200°F) and should not be used for final cure cycles, as the film may bond to the structure.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 50.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2600 psi
Elongation at Break 120 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °C
 
Descriptive Properties
ColorMatte white
Yield28 m2/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman 9921 PET Film
Armacell ArmaFORM® PET Foil 70
Eastman 9921P PET Film
Chengdu Polyster PET Film PET Films/Sheets
DuPont Teijin Films Melinex® HC-1 Planarised PET film

PCYTED275 / 180577

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.