MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SCG Chemicals EL-Lene™ H2001WC High Density Polyethylene Wire & Cable Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); HDPE, Fiber Grade

Material Notes: Key Characteristics:Excellent environmental stress cracking resistance (ESCR), high mechanical properties, high speed extrusion

Recommended Applications:

  • Jacketing of fiber optical cables
  • Jacketing of power cables

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.952 g/ccASTM D1505
Density of Compound 0.963 g/ccASTM D1505
Environmental Stress Crack Resistance >= 10000 hour
@Temperature 50.0 °C
F0, 25% Igepal; ASTM D1693
Oxidative Induction Time (OIT) >= 70 min
@Temperature 200 °C
ASTM D3895
Carbon Black Loading 2.5 %ASTM D4218
Melt Flow 0.13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ASTM D2240
Tensile Strength at Break 33.0 MPaASTM D638
Tensile Strength, Yield 240 kg(f)/cm²ASTM D638
Elongation at Break 840 %ASTM D638
Flexural Modulus >= 10000 kg(f)/cm²ASTM D790
Izod Impact, Notched 21.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.564ASTM D1531
Dielectric Strength 20.0 kV/mmASTM D149
Dissipation Factor 0.0050ASTM D1531
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -75.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global BM-3245-PC High Density Polyethylene, Pipe Extrusion Grade
ExxonMobil HPA 020 Wire & Cable High Density Polyethylene Resin
LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound
LyondellBasell Petrothene® KR92828 High Density Polyethylene
Dow HDPE 30460M High Density Polyethylene

PSCGC914 / 120668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.