MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American White Oak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Due to acidic nature, may stain when in contact with iron under damp conditions. May also corrode metals. Ring-Porous Hardwood. Least easy to work with hand tools. Excellent steam bending, excellent planing, fair shaping. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Durable (15 to 25 years)
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Furniture, cabinet work. Tight cooperage

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Quercus alba; Q.spp.; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.600 g/ccOven Dry Weight/Unseasoned Volume
 62.0 lb/ft³Unseasoned*
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 4700 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 5000 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 6000 NSide
Tensile Strength, Ultimate 5.50 MPaPerpendicular to Grain
 770 psiPerpendicular to Grain*
Modulus of Rupture 0.105 GPaIn Bending
 8.30 ksiStatic Bending*
Flexural Yield Strength 56.5 MPaBending stress at proportional limit
 4700 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 12.28 - 12.4 GPaIn Bending
 1250 ksiStatic Bending*
Compressive Strength 9.10 MPaPerpendicular to Grain
 48.3 - 51.0 MPaParallel to Grain
 830 psiPerpendicular to Grain*
 2990 psiParallel to Grain*
 3560 psiMax Crushing Strength Parallel to Grain*
Poissons Ratio 0.036µTL, 12% Moisture Content
 0.074µRL, 12% Moisture Content
 0.30µTR, 12% Moisture Content
 0.369µLR, 12% Moisture Content
 0.428µLT, 12% Moisture Content
 0.618µRT, 12% Moisture Content
Machinability 50 %Medium Relative to Other Wood
Shear Strength 13.5 MPaOrientation Unknown
 1250 psiParallel to Grain*
Impact 4.2in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 10700psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 1.08 in-lb/in³Static Bending*
Work to Maximum Load 11.5 in-lb/in³Static Bending*
Toughness 35.0 JTangential
 38.4 JRadial
Cleavage 67.0 kN/mRadial surface of failure, Unseasoned*
 80.0 kN/mTangential surface of failure, Unseasoned*
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.90 µm/m-°C
@Temperature 20.0 °C
Axial. Typical value for Oak.
 11.1 µm/m-°C
@Temperature 20.0 °C
Radial; Typical value for Oak.
 54.4 µm/m-°C
@Temperature 20.0 °C
Tangential. Typical value for Oak.
Shrinkage 5.3 %Radial; Green to Zero Moisture
 9.6 %Tangential; Green to Zero Moisture
 18.9 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorPale yellow to mid-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Red Oak Wood
European White Oak Wood
European Oak Wood
European Red Oak Wood
North American Northern Red Oak Wood

PTSAW / 71306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.