MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
C.O.I.M. LARIPUR® LPR7018 Plasticized Ester Polyurethane
Categories: Polymer; Thermoplastic; Polyester, TP; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 15 and 19 Plasticized Ester: These products are esters containing a small amount of a low migrating plasticizer. They are soft grade TPU mainly developed for the footwear industry. These two series of LARIPUR® combine the properties of polyurethane with those of rubber.
Despite their low hardness, they exhibit fast processing cycles. Products belonging to Series 18 are fully transparent while those of Series 15 are opaque. Both exhibit a very good adhesion to most two component PU systems without any pre-treatment.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ASTM D2240
Tensile Strength, Yield 36.0 MPaASTM D412
Elongation at Break 830 %ASTM D412
50% Modulus 0.00220 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.00320 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00580 GPa
@Strain 300 %
ASTM D412
Tear Strength 60.0 kN/mASTM D624
Abrasion 40mm3, Abrasion Loss; DIN 53516
Compression Set 48 %
@Temperature 70.0 °C
Method B, 22 hours; ASTM D395
 24 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 65.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
FeaturesTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR7015 Plasticized Ester Polyurethane
C.O.I.M. LARIPUR® LPR8020 Standard Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR5850 Modified Ester Polyurethane

PCOIM022 / 28625

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.