MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexPly® M49 is a 120°C curing toughened epoxy matrix with good impact resistance suitable for use in performance cars. The matrix is highly tolerant of a wide variety of production techniques and equipment making it easy to process.

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/cc
Viscosity >= 5000 cP
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 95.0 °CWet
 120 °CAfter 120°C, 60 min cure dry
 
Processing PropertiesOriginal ValueComments
Gel Time 12.0 - 14.0 min
@Temperature 120 °C
Shelf Life 12.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® M10E Epoxy Resin
Hexcel® HexPly® F593 Epoxy Resin
Hexcel® HexPly® F522 Epoxy Resin
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix

PHEXC194 / 98665

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.