MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 5502 BZ HDPE injection blow molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Applications: Cosmetics and toiletries, pharmaceuticals, specialty containers, food packaging

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D 792
Environmental Stress Crack Resistance 35 hourASTM D1693 cond. B 10% lgepal
 50 hourASTM D1693 cond. B 100% lgepal
Melt Flow 0.35 g/10 min
@Load 2.16 kg
ASTM D 1238
High Load Melt Index 30 g/10 min
@Load 21.6 kg
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4000 psiASTM D 638 type IV
Elongation at Break >= 600 %ASTM D 638 type IV
Flexural Modulus 200000 psiASTM D 790
 
Thermal PropertiesOriginal ValueComments
Melting Point 264 °FASTM D3417

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
Total 5502 R3 High Density Polyethylene - Blow Molding
SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding
Chevron Phillips Marlex® 9503H HDPE Blow Molding Resin
Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE

PFINAP144 / 38727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.