MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin NEOFLON® NP-21 FEP Pellets  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP); Fluorinated Ethylene Propylene (FEP), Molded/Extruded; Perfluoroalkoxy (PFA)

Material Notes: NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.

Processing Methods: Extrusion molding, injection molding.

Applications: Suited to high speed extrusion and injection molding.

Information provided by Daikin Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.12 - 2.17 g/ccASTM D792
Bulk Density 1.20 g/cc
Water Absorption <= 0.010 %
@Thickness 8.50 mm,
Time 86400 sec
ASTM D570
Oxygen Transmission 320 cc-mm/m²-24hr-atmat 25°C
Nitrogen Transmission 104 cc-mm/m²-24hr-atmat 25°C
Viscosity 4.00e+6 - 4.00e+7 cP
@Temperature 380 °C
Melt viscosity
Linear Mold Shrinkage 0.030 - 0.060 cm/cm
Melt Flow 5.5 - 7.5 g/10 min
@Load 5.00 kg,
Temperature 372 °C
Deformation 3.0 %13.7 MPa load, at 25°C, 24 hrs; ASTM D621
 5.0 %6.7 MPa load, at 100°C, 24 hrs; ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55
Tensile Strength at Break 19.0 - 22.0 MPaASTM D638
Elongation at Break 250 - 330 %ASTM D638
Tensile Modulus 0.343 GPaASTM D638
Flexural Modulus 0.539 - 0.637 GPaASTM D790
Compressive Strength 5.00 - 6.00 MPa
@Temperature 25.0 °C
1% deformation; ASTM D695
Izod Impact, Unnotched NBASTM D256
Coefficient of Friction 0.040 - 0.060
Coefficient of Friction, Static 0.050Coated-steel surface
Taber Abrasion, mg/1000 Cycles <= 6.0Calculated using estimated density, 9.8 N load, cs-10 wheel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.00e+18 ohm-cmASTM D257
Dielectric Constant 2.1
@Frequency 1000 Hz
ASTM D150
 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 - 24.0 kV/mm
@Thickness 3.20 mm
Short time; ASTM D149
Dissipation Factor 0.000060
@Frequency 1000 Hz
ASTM D150
 0.00050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 83.0 - 105 µm/m-°C
@Temperature 23.0 - 60.0 °C
ASTM D696
Thermal Conductivity 0.250 W/m-KASTM C177
Melting Point 260 - 270 °C
Maximum Service Temperature, Air 200 °CContinuous use
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Descriptive Properties
Chemical ResistanceExcellent
Contact Angle114Angle to level
WeatherabilityExcellent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® FEP FR5020 Fluoropolymer Resin
Chemours Teflon® FEP CX5010 Fluoropolymer Resin
Chemours Teflon® FEP FR5030 Fluoropolymer Resin
Daikin NEOFLON® NP-3000 FEP Pellets
Chemours Teflon® FEP CJ-95 Fluoropolymer Resin

PDAIK114 / 29406

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.