MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Anderman Ceramics EREH99 Hafnium Oxide, High Purity
Categories: Ceramic; Oxide

Material Notes: Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance metal melting, oxygen sensors, and semiconductor applications. Products are offered in a wide variety of shapes and sizes.

Key Words: HfO2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.00 g/cc
Open Porosity <= 1.0 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 2812 °C
 
Component Elements PropertiesOriginal ValueComments
HfO2 99.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Anderman Ceramics EM80P Corundum
Anderman Ceramics EREH97Y Hafnium Oxide, Yttrium Oxide-Stabilized
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Anderman Ceramics EA95 Sintered Alumina, 95%
Advanced Ceramics ALC 1082 (C-786) Alumina

CANDER19 / 104654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.