MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe LSS™ 4140 Alloy Steel (AISI 4140)
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; Medium Carbon Steel; Tool Steel

Material Notes: TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed condition at a hardness less than or equal to 217 HBW. TLS 4142HT is a similar steel which is sold prehardened to 28 to 32 HRC (269 to 302 HBW). Pieces of TLS 4142HT which are greater than about 3 inches (76.2mm) in thickness typically exhibit a lower hardness in the central region of the cross section. Typical applications for these steels include break dies, bending dies, support tooling, die holders, gears, flanges, collets, arbors, spindles, axles, clutch parts, forming rolls, wrenches and other hand tools, and various machine tool components.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.83 g/cc
Density 0.283 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 27Oil Quenched from 843°C; 649°C Temper Temperature
 60Oil Quenched from 843°C; As Quenched
Modulus of Elasticity 29000 ksi
Machinability 60 - 65 %1% Carbon Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.22 µm/m-°C
@Temperature 21.0 - 100 °C
Thermal Conductivity 37.7 W/m-K
@Temperature 300 °C
 42.3 W/m-K
@Temperature 200 °C
 42.7 W/m-K
@Temperature 100 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 °CCritical Temperaure Mf
 343 °CCritical Temperaure Ms
 680 °CCritical Temperaure Ar1
 732 °CCritical Temperaure Ac1
 743 °CCritical Temperaure Ar3
 804 °CCritical Temperaure Ac3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 1.0 %
Iron, Fe 97.15 %
Manganese, Mn 1.0 %
Molybdenum, Mo 0.20 %
Silicon, Si 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
Latrobe LSS™ 4142 Alloy Steel (AISI 4142)
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 100 mm (4 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 25 mm (1 in.) round

NTIMK122 / 19469

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.