MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: (PC+PBT)-blend, 20% Glass fiber reinforced, easy release, injection molding. Makroblend UT4045G offers a high stiffness, excellent chemical resistance, good flowability and exceptional dimensional stability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183-1
Filler Content 20 %20 %Method A; b.o. ISO 3451-1
Moisture Absorption at Equilibrium 0.15 %0.15 %ISO 62
Water Absorption at Saturation 0.30 %0.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in150x105x3 mm; 260 °C / MT 80 °C; 600 bar; b.o. ISO 2577
 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inb.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in150x105x3 mm; 260 °C / MT 80 °C; 600 bar; b.o. ISO 2577
Melt Flow 42 g/10 min
@Load 5.00 kg,
Temperature 260 °C
42 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 90.0 MPa13100 psiISO 2039-1
Tensile Strength at Break 100 MPa14500 psi5 mm/min; ISO 527-1,-2
Tensile Strength, Yield 100 MPa14500 psi50 mm/min; ISO 527-1,-2
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527-1,-2
 3.0 %3.0 %Nominal, 5 mm/min; ISO 527-1,-2
Elongation at Yield 3.0 %3.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 6.50 GPa943 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 160 MPa23200 psi2 mm/min; ISO 178
Flexural Modulus 6.10 GPa885 ksi2 mm/min; ISO 178
Flexural Strain at Yield 3.0 %3.0 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
Izod Impact, Unnotched (ISO)  35.0 kJ/m²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 180-U
 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180-U
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mm
@Thickness 1.00 mm
838 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0013
@Frequency 100 Hz
0.0013
@Frequency 100 Hz
IEC 60250
 0.0144
@Frequency 1e+6 Hz
0.0144
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V175 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 35.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
19.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75-1,-2
Vicat Softening Point 140 °C
@Load 5.10 kg
284 °F
@Load 11.2 lb
120°C/h; ISO 306
Shrinkage <= 0.10 %<= 0.10 %post-shrinkage; b.o. ISO 2577
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection molding; ISO 294
Mold Temperature 70.0 °C158 °FInjection molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® UT5205 PC/PBT Blend
Covestro Makroblend® UT5207 PC/PBT Blend
Polykemi AB POLYlux 3809S F20 PC/PBT-Blend, Glass Fiber-Reinforced
A. Schulman Lucent GPCB-110 Polycarbonate+PBT, 10% Glass Fiber Reinforced
LG Chemical Lupox® LW5102F PBT+PC+GF10%

PB09659 / 150791

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.