MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hong Kun Group UV 234 UV Absorber
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: UV 234 is a high molecular weight ultraviolet light absorber (UVA) of the hydroxyl phenyl benzotriazole class, imparting outstanding light stability to polymers usually processed at high temperatures such as polycarbonate, polyesters, polyacetal, polyamides, polyphenylene sulfide, polyphenylene oxide, aromatic copolymers, thermoplastic polyurethane and polyurethane fibers, where loss of UVA is not tolerated as well as for polyvinylchloride, styrene homo- and copolymers. Applications include molded articles, films, sheets and fibers.

Chemical Name: 2-(2H-benzotriazol-2-yl)-4,6- bis(1-methyl-1-phenylethyl) phenol

CAS No. 70321-86-7

All information provided by Hongkun Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.50 %
Molecular Weight 447.3 g/mol
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 137 - 141 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 97 %
@Wavelength 460 nm
 >= 98 %
@Wavelength 500 nm
 
Descriptive Properties
Appearancelight yellow powder/granule
Purity (%)>= 99

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTOWAX® SH 105 Powder Paraffin Wax
Lithium Nitrate, LiNO3
Overview of materials for Polycarbonate, 10% Glass Filled
Hong Kun Group UV 329 UV Absorber
Heraeus Clevios™ P T2 Conductive Sulfonate Polymer for Antistatic Coatings

PHONGK003 / 86304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.