MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical Lucet® N109 Acetal Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Polyacetal; Polyoxymethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Water Absorption 0.22 %24 hours at 73°F; ASTM D570
Linear Mold Shrinkage 0.018 - 0.021 cm/cmASTM D955
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 82ASTM D785
Tensile Strength, Yield 620 kg(f)/cm²23°C; 50% RH; ASTM D638
Elongation at Break 65 %ASTM D638
Flexural Yield Strength 910 kg(f)/cm²23°C; 50% RH; ASTM D570
Flexural Modulus 26000 kg(f)/cm²23°C; 50%RH; ASTM D570
Izod Impact, Notched 7.00 kg-cm/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 240 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 160 °CASTM D648
Flammability, UL94 HB
@Thickness 0.7937 mm
UL94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 320 - 356 °F
Middle Barrel Temperature 356 - 392 °F
Front Barrel Temperature 374 - 419 °F
Nozzle Temperature 374 - 419 °F
Melt Temperature 392 - 437 °F
Mold Temperature 140 - 212 °F
Drying Temperature 194 - 230 °F
Dry Time 3 - 6 hour
Screw Speed 50 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acetal Homopolymer, Unreinforced
PTS Trilac® ABS-HF5500 High Flow ABS Resin
Avient Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE)
Chi Mei Polylac® PA-717C ABS

PLBA00 / 50356

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.