MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MetalTek MTEK 70-30 UNS C96400 Nickel-Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Nickel Alloy

Material Notes: Information provided by MetalTek

Key Words: Cast UNS C96400; Cast Grade C96400; Cast ASTM B369; Military MIL-C-20159
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³Based on UNS number
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 140140
Tensile Strength, Ultimate >= 415 MPa>= 60200 psi
Tensile Strength, Yield >= 220 MPa>= 31900 psi
Elongation at Break >= 20 %>= 20 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Copper, Cu 63.35 - 71.25 %63.35 - 71.25 %
Iron, Fe 0.25 - 1.5 %0.25 - 1.5 %
Manganese, Mn <= 1.5 %<= 1.5 %
Nickel, Ni 28 - 32 %28 - 32 %
Niobium, Nb (Columbium, Cb) 0.50 - 1.0 %0.50 - 1.0 %
Silicon, Si <= 0.50 %<= 0.50 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Nickel 70/Copper 30 Alloy
MetalTek MTEK A Cast UNS N04020 Nickel-Copper Alloy
MetalTek MTEK B Cast UNS N24030 Nickel-Copper Alloy
UNS C96400, Copper Casting Alloy
Special Metals MONELĀ® 404 Copper-Nickel Alloy

NMETEK142 / 18392

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.