MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dymax 3073 Solvent-Free Plastic Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes:
Solvent-Free Adhesives for Plastic Assembly in Seconds
Dymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide variety of engineering plastics. Curing in seconds upon exposure to UV/visible light, these resins are ideal for bonding transparent surfaces and for potting, sealing, and coating applications. Ultra Light-Weld adhesives and sealants cure upon exposure to UV and/or visible light and are perfect for UV blocked and tinted plastics. Light Weld products cure upon exposure to UV light.

Environmentally responsible, solvent free adhesives reduce regulatory compliance cost, and encourage worker acceptance of the assembly process.

Dymax 3073 Solvent-Free Plastic Adhesive
Key Substrates: PBT/Valox® (primary), Metal, Glass, PVC, SAN, PS, K-resin® Typical Use: Fastest cure, flexible

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 30000 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 3000 psi
Elongation at Break 80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
LyondellBasell Plexar® PX5125 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
Silon Tabond 2001 Adhesive Resin
ExxonMobil LD 145.PX Packaging Resin
Covestro Bayhydrol® A 145 Polyurethane Coating

PDYYMAX13 / 34997

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.