MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials TC1050 Encapsulated Thermal Pyrolytic Graphite (TPG)
Categories: Carbon; Graphite

Material Notes: GE Advanced Ceramics has developed a family of thermal materials based upon its high conductivity thermal pyrolytic graphite (TPG) material. TPG is a unique form of pyrolytic graphite manufactured by the decomposition of a hydrocarbon gas in a high vacuum furnace. Referred to as TC1050, these macrocomposite materials offer both high conductivity, low density, and low thermal expansion properties. TC1050 consists of a TPG core encapsulated within a structural shell. The TPG provides a highly conductive path while the encapsulation material provides the structure (strength, stiffness, and coefficient of thermal expansion). Chemical isolation and electrical insulation of the aluminum from the graphite resistive element for PBN/G evaporators permit electrical resistance stability and consistency throughout their long life. This guarantees absolute flash-to-flash temperature repeatability, total aluminum evaporation and thickness (Q-value) consistency of the deposited layer. Encapsulant materials include 6061 aluminum, OFHC copper, and graphite/polymer composites.

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Momentive Performance Materials "PG" Pyrolytic Graphite
Pyrolytic Graphite, Low Temperature Isotropic (LTI)
Momentive Performance Materials Pyrolytic Graphite (PG) Coating
Momentive Performance Materials HOPG Graphite Monochromator

CADV80 / 454

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.